In the present work we report an anelastic spectroscopy study of pure FeCO3 (siderite) and of carbon steel samples covered by siderite films. Uncovered steel samples have also been investigated for reference. The siderite shows two relaxation processes below room temperature, at about 220 K and 140 K, while the covered steel sample displays only the peak at lower temperature. The presence of such a relaxation can be used to monitor the deposition of siderite. (C) 2009 Elsevier B.V. All rights reserved.
Anelastic spectroscopy study of iron carbonate scales from CO2 corrosion of steel / O., Palumbo; A., Paolone; Rispoli, Pasquale; Cantelli, Rosario; G., Cannelli; Nesic, ; B. J., Molinas; P. P., Zonta. - In: MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING. - ISSN 0921-5093. - 521-22:(2009), pp. 343-346. (Intervento presentato al convegno 15th International Conference on Internal Friction and Mechanical Spectroscopy (ICIFMS-15) tenutosi a Perugia, ITALY nel JUL 20-25, 2008) [10.1016/j.msea.2008.09.091].
Anelastic spectroscopy study of iron carbonate scales from CO2 corrosion of steel
RISPOLI, PASQUALE;CANTELLI, Rosario;
2009
Abstract
In the present work we report an anelastic spectroscopy study of pure FeCO3 (siderite) and of carbon steel samples covered by siderite films. Uncovered steel samples have also been investigated for reference. The siderite shows two relaxation processes below room temperature, at about 220 K and 140 K, while the covered steel sample displays only the peak at lower temperature. The presence of such a relaxation can be used to monitor the deposition of siderite. (C) 2009 Elsevier B.V. All rights reserved.I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.