This study presents a comprehensive risk assessment of battery vent gas (BVG) from lithium-ion cells, focusing on its dynamic composition and laminar burning velocity (Su). It highlights lithium titanate (LTO) cells, which use Li4Ti5O12 anode, and compares them with NMC, NCA, and LFP chemistries. LTO cells improved safety by mitigating lithium plating and dendrite growth, key causes of internal short circuits and thermal runaway (TR). BVG composition evolves significantly during TR and depends on cell chemistry and state of charge (SoC), affecting combustion behaviour. BVG composition and Su were quantified during different stages of thermal abuse for cells with various chemistries and SoC (50% and 100%). A lab-scale setup with FT-IR and Micro-GC identified gases such as H2, CO, CO2, CH4, HF, and organic carbonates. Additional analyses (FT-IR) identified unburned species, while CHEMKIN-Premix calculated Su and sensitivity factors. Results show that LTO and LFP cells are safer under thermal abuse. At 100% SoC, NMC produced the most hazardous BVG, with higher hydrogen and the highest Su. At 50% SoC, TR was suppressed for LTO and LFP cells. These findings provide key insights into combustion dynamics and support improved mitigation of fire and explosion hazards in lithium-ion batteries.

Flammability of lithium-ion battery vent gas: The combined effect of cell chemistry, state of charge, and failure phase / Russo, P., Ubaldi, S.. - In: FIRE SAFETY JOURNAL. - ISSN 0379-7112. - 165:(2026). [10.1016/j.firesaf.2026.104930]

Flammability of lithium-ion battery vent gas: The combined effect of cell chemistry, state of charge, and failure phase

Russo, Paola
Primo
Funding Acquisition
;
Ubaldi, Sofia
Ultimo
Writing – Original Draft Preparation
2026

Abstract

This study presents a comprehensive risk assessment of battery vent gas (BVG) from lithium-ion cells, focusing on its dynamic composition and laminar burning velocity (Su). It highlights lithium titanate (LTO) cells, which use Li4Ti5O12 anode, and compares them with NMC, NCA, and LFP chemistries. LTO cells improved safety by mitigating lithium plating and dendrite growth, key causes of internal short circuits and thermal runaway (TR). BVG composition evolves significantly during TR and depends on cell chemistry and state of charge (SoC), affecting combustion behaviour. BVG composition and Su were quantified during different stages of thermal abuse for cells with various chemistries and SoC (50% and 100%). A lab-scale setup with FT-IR and Micro-GC identified gases such as H2, CO, CO2, CH4, HF, and organic carbonates. Additional analyses (FT-IR) identified unburned species, while CHEMKIN-Premix calculated Su and sensitivity factors. Results show that LTO and LFP cells are safer under thermal abuse. At 100% SoC, NMC produced the most hazardous BVG, with higher hydrogen and the highest Su. At 50% SoC, TR was suppressed for LTO and LFP cells. These findings provide key insights into combustion dynamics and support improved mitigation of fire and explosion hazards in lithium-ion batteries.
2026
Battery vent gas; Kinetic mechanism; Laminar burning velocity; Lithium-ion batteries; LTO; Premixed flame; Thermal runaway
01 Pubblicazione su rivista::01a Articolo in rivista
Flammability of lithium-ion battery vent gas: The combined effect of cell chemistry, state of charge, and failure phase / Russo, P., Ubaldi, S.. - In: FIRE SAFETY JOURNAL. - ISSN 0379-7112. - 165:(2026). [10.1016/j.firesaf.2026.104930]
File allegati a questo prodotto
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11573/1781593
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 0
  • ???jsp.display-item.citation.isi??? 0
social impact