Lithium-ion batteries (LIBs) are employed in a range of devices due to their high energy and power density. However, the increased power density of LIBs raises concerns regarding their safety when subjected to external abuse. The thermal behavior is influenced by a number of factors, i.e., the state of charge (SoC), the cell chemistry and the abuse conditions. In this study, three distinct cylindrical Li-ion cells, i.e., lithium nickel cobalt aluminum oxide (NCA), lithium titanate oxide (LTO), and lithium iron phosphate (LFP), were subjected to thermal abuse (heating rate of 5 °C/min) in an air flow reactor, with 100% SoC. Venting and thermal runaway (TR) were recorded in terms of temperature and pressure, while the emitted products (gas, solid, and liquid) were subjected to analysis by FT-IR and ICP-OES. The concentrations of the toxic gases (HF, CO) are significantly in excess of the Immediate Danger to Life or Health Limit (IDLH). Furthermore, it is observed that the solid particles are the result of electrode degradation (metallic nature), whereas the liquid aerosol is derived from the electrolyte solvent. It is therefore evident that in the event of a LIB fire, in order to enhance the safety of the emergency responders, it is necessary to use appropriate personal protective equipment (PPE) in order to minimize exposure to toxic substances, i.e., particles and aerosol.
Toxicity Assessment of Gas, Solid and Liquid Emissions from Li-Ion Cells of Different Chemistry Subjected to Thermal Abuse / Ubaldi, Sofia; Russo, Paola. - In: ENERGIES. - ISSN 1996-1073. - 17:17(2024). [10.3390/en17174402]
Toxicity Assessment of Gas, Solid and Liquid Emissions from Li-Ion Cells of Different Chemistry Subjected to Thermal Abuse
Ubaldi, SofiaPrimo
;Russo, Paola
Ultimo
2024
Abstract
Lithium-ion batteries (LIBs) are employed in a range of devices due to their high energy and power density. However, the increased power density of LIBs raises concerns regarding their safety when subjected to external abuse. The thermal behavior is influenced by a number of factors, i.e., the state of charge (SoC), the cell chemistry and the abuse conditions. In this study, three distinct cylindrical Li-ion cells, i.e., lithium nickel cobalt aluminum oxide (NCA), lithium titanate oxide (LTO), and lithium iron phosphate (LFP), were subjected to thermal abuse (heating rate of 5 °C/min) in an air flow reactor, with 100% SoC. Venting and thermal runaway (TR) were recorded in terms of temperature and pressure, while the emitted products (gas, solid, and liquid) were subjected to analysis by FT-IR and ICP-OES. The concentrations of the toxic gases (HF, CO) are significantly in excess of the Immediate Danger to Life or Health Limit (IDLH). Furthermore, it is observed that the solid particles are the result of electrode degradation (metallic nature), whereas the liquid aerosol is derived from the electrolyte solvent. It is therefore evident that in the event of a LIB fire, in order to enhance the safety of the emergency responders, it is necessary to use appropriate personal protective equipment (PPE) in order to minimize exposure to toxic substances, i.e., particles and aerosol.I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.