The development of Li/sulfurized polyacrylonitrile (SPAN) batteries requires electrolytes that can form stable electrolyte/electrode interphases simultaneously on lithium-metal anodes (LMAs) and SPAN cathodes. Herein, a low-flammability locally concentrated ionic liquid electrolyte (LCILE) employing monofluorobenzene (mFBn) as the diluent is proposed for Li/SPAN cells. Unlike non-solvating diluents in other LCILEs, mFBn partially solvates Li+, decreasing the coordination between Li+ and bis(fluorosulfonyl)imide (FSI-). In turn, this triggers a more substantial decomposition of FSI- and consequently results in the formation of a solid electrolyte interphase (SEI) rich in inorganic compounds, which enables a remarkable Coulombic efficiency (99.72%) of LMAs. Meanwhile, a protective cathode electrolyte interphase (CEI), derived mainly from FSI- and organic cations, is generated on the SPAN cathodes, preventing the dissolution of polysulfides. Benefiting from the robust interphases simultaneously formed on both the electrodes, a highly stable cycling of Li/SPAN cells for 250 cycles with a capacity retention of 71% is achieved employing the LCILE and only 80% lithium-metal excess.
Locally concentrated ionic liquid electrolyte with partially solvating diluent for lithium/sulfurized polyacrylonitrile batteries / Liu, Xu; Diemant, Thomas; Mariani, Alessandro; Dong, Xu; Di Pietro, Maria Enrica; Mele, Andrea; Passerini, Stefano. - In: ADVANCED MATERIALS. - ISSN 0935-9648. - 34:49(2022). [10.1002/adma.202207155]
Locally concentrated ionic liquid electrolyte with partially solvating diluent for lithium/sulfurized polyacrylonitrile batteries
Passerini, Stefano
2022
Abstract
The development of Li/sulfurized polyacrylonitrile (SPAN) batteries requires electrolytes that can form stable electrolyte/electrode interphases simultaneously on lithium-metal anodes (LMAs) and SPAN cathodes. Herein, a low-flammability locally concentrated ionic liquid electrolyte (LCILE) employing monofluorobenzene (mFBn) as the diluent is proposed for Li/SPAN cells. Unlike non-solvating diluents in other LCILEs, mFBn partially solvates Li+, decreasing the coordination between Li+ and bis(fluorosulfonyl)imide (FSI-). In turn, this triggers a more substantial decomposition of FSI- and consequently results in the formation of a solid electrolyte interphase (SEI) rich in inorganic compounds, which enables a remarkable Coulombic efficiency (99.72%) of LMAs. Meanwhile, a protective cathode electrolyte interphase (CEI), derived mainly from FSI- and organic cations, is generated on the SPAN cathodes, preventing the dissolution of polysulfides. Benefiting from the robust interphases simultaneously formed on both the electrodes, a highly stable cycling of Li/SPAN cells for 250 cycles with a capacity retention of 71% is achieved employing the LCILE and only 80% lithium-metal excess.File | Dimensione | Formato | |
---|---|---|---|
Liu_Locally_2022.pdf
accesso aperto
Note: full paper
Tipologia:
Versione editoriale (versione pubblicata con il layout dell'editore)
Licenza:
Creative commons
Dimensione
6.57 MB
Formato
Adobe PDF
|
6.57 MB | Adobe PDF |
I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.