The effect of a preliminary acid leaching for the recovery of gold by thiourea from printed circuit boards (PCBs) of spent mobile phones, was investigated. Preliminary leaching is aimed to recover copper in the leachate that would compete with gold in the successive leaching of the residue with thiourea, thus preventing the formation of the gold-thiourea complex. Two hydrometallurgical routes were tested for the recovery of copper first, and gold after. The first one was based on a two-step leaching that utilizes sulfuric acid and hydrogen peroxide in the preliminary leaching and then thiourea for the recovery of gold in the successive leaching: A copper and gold recovery of 81% and 79% were obtained, respectively. In the second route, nitric acid was used: 100% of copper was recovered in the leachate and 85% of gold in the thiourea successive leaching. The main operative parameters, namely thiourea and ferric sulphate concentrations, leach time, liquid-solid ratio, and temperature were studied according to a factorial plan strategy. A flowsheet of the processes was proposed, and a mass balance of both routes was obtained. Finally, qualitative considerations on the technical and economic feasibility of the different routes were made.

Effect of acid leaching pre-treatment on gold extraction from printed circuit boards of spent mobile phones / Ippolito, N. M.; Medici, F.; Pietrelli, L.; Piga, L. - In: MATERIALS. - ISSN 1996-1944. - 14:2(2021), pp. 1-15. [10.3390/ma14020362]

Effect of acid leaching pre-treatment on gold extraction from printed circuit boards of spent mobile phones

Medici, F.
Secondo
Membro del Collaboration Group
;
Piga, L
Ultimo
Membro del Collaboration Group
2021

Abstract

The effect of a preliminary acid leaching for the recovery of gold by thiourea from printed circuit boards (PCBs) of spent mobile phones, was investigated. Preliminary leaching is aimed to recover copper in the leachate that would compete with gold in the successive leaching of the residue with thiourea, thus preventing the formation of the gold-thiourea complex. Two hydrometallurgical routes were tested for the recovery of copper first, and gold after. The first one was based on a two-step leaching that utilizes sulfuric acid and hydrogen peroxide in the preliminary leaching and then thiourea for the recovery of gold in the successive leaching: A copper and gold recovery of 81% and 79% were obtained, respectively. In the second route, nitric acid was used: 100% of copper was recovered in the leachate and 85% of gold in the thiourea successive leaching. The main operative parameters, namely thiourea and ferric sulphate concentrations, leach time, liquid-solid ratio, and temperature were studied according to a factorial plan strategy. A flowsheet of the processes was proposed, and a mass balance of both routes was obtained. Finally, qualitative considerations on the technical and economic feasibility of the different routes were made.
2021
printed circuit boards; spent mobile phones; thiourea; precious metals; hydrometallurgy; factorial plans
01 Pubblicazione su rivista::01a Articolo in rivista
Effect of acid leaching pre-treatment on gold extraction from printed circuit boards of spent mobile phones / Ippolito, N. M.; Medici, F.; Pietrelli, L.; Piga, L. - In: MATERIALS. - ISSN 1996-1944. - 14:2(2021), pp. 1-15. [10.3390/ma14020362]
File allegati a questo prodotto
File Dimensione Formato  
Ippolito_Effect-acid-leaching_2021.pdf

accesso aperto

Tipologia: Versione editoriale (versione pubblicata con il layout dell'editore)
Licenza: Creative commons
Dimensione 1.66 MB
Formato Adobe PDF
1.66 MB Adobe PDF

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11573/1480749
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 24
  • ???jsp.display-item.citation.isi??? 23
social impact